Selectpart Standard series friction pads to fit the following Montalvo brakes and clutches
- HP-Series High Performance Dual Disc Brakes equipped with Dual S friction modules
- Standard-Series Dual Disc Brakes equipped with Dual S friction modules
- HPS-Series High Performance Single Disc Brakes equipped with HPS friction modules
- HPS-Series High Performance Single Disc Clutches equipped with HPS friction modules
- M-Caliper Series brakes equipped with M-Caliper friction modules
H302G is the standard pad supplied with all Montalvo Standard pad equipped tension brakes and clutches.
Selectpart Standard Series friction pads are 3.25" (82.6mm) diameter.
The following chart details available friction pads based on Coefficient of Friction* and material composition.
Selectpart # | Montalvo # | COF |
Edge | Grooved | Material | Description | ID # (on_back) | SDS | Price Request |
---|---|---|---|---|---|---|---|---|---|
H302G | 4512G | High | None | Yes | Carbon base with various phenolic fillers and bonding agents. | Standard material for most applications. Low cost. One of the best pads for noise problems. | H302G | Price Request | |
H302GT | 4512GT Anti-Sql | High | None | Yes | Carbon base with various phenolic fillers and bonding agents. | With anti-squeal noise reduction. Standard material for most applications. Low cost. One of the best pads for noise problems. | H302G | Price Request | |
H301G | 4511G | High | Orange | Yes | Carbon base with various phenolic fillers and bonding agents. | High torque, normal speed. Tends to glaze at intermediate to high temps and low pressures. May be unstable above 350F. High propensity to make noise. | H301G | Price Request | |
H301GT |
4511GT Anti-Sql |
High | Orange | Yes | Carbon base with various phenolic fillers and bonding agents. | With anti-squeal noise reduction. High torque, normal speed. Tends to glaze at intermediate to high temps and low pressures. May be unstable above 350F. | H301G | Price Request | |
H306 | 4514 | High | None | No | Carbon base with various phenolic fillers and bonding agents. | High torque, low temp. COF fades above 250F. Wears faster but may be suitable for some noise problems. |
H306 | Price Request | |
H300G | 4011G | High | Blue | Yes | Carbon base with various phenolic fillers and bonding agents. | General use. Longer pad life typical. Stable COF at elevated temps. May glaze at high temp, low pressure, low speed. High propensity for noise. | H300G | Price Request | |
H313 |
Kevlar + | Medium | None (Solid Tan Pad) | No | Kevlar base with carbon base backing, phenolic fillers and bonding agents | Stable COF at most temps and pressures. Good for high wear applications (HP26) with high power dissipation requirements. | H313 | Price Request | |
M201G | 3012G | Medium | Yellow | Yes | Carbon base with various phenolic fillers and bonding agents. | General use. Med-friction, med torque. May glaze at high temps/low pressures. Unstable above 350F. One of the best pads for noise problems. May not be sufficient when changing from 3011 due to lower overall coefficient. | M201G | Price Request | |
M201GT | 3012GT Anti-Sql | Medium | Yellow | Yes | Carbon base with various phenolic fillers and bonding agents. | General use. Med-friction, med torque. May glaze at high temps/low pressures. Unstable above 350F. One of the best pads for noise problems. May not be sufficient when changing from 3011 due to lower overall coefficient. | M201G | Price Request | |
M200G | 3011G | Medium | Green | Yes | Carbon base with various phenolic fillers and bonding agents. | General use. Low cost, med friction, med torque. May glaze at high temp, low pressure. Unstable above 350F. High propensity to make noise. |
M200G | Price Request | |
M203 | 3001 | Medium | None (Solid Green Pad) | No | Teflon with fiberglass, fillers & bonding agents | High speed, low temp, low torque. Stable COF at low temps. Unstable above 200F. Very quiet. |
M203 | Price Request | |
L100G | 1011G | Low | Red | Yes | Carbon base with various phenolic fillers and bonding agents | General use. Low friction, low torque. May glaze at high temps and low operating pressures. Unstable above 350°F. | L100G | Price Request |